this post was submitted on 09 Aug 2024
17 points (100.0% liked)

3DPrinting

15250 readers
30 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

I have a K1 Max and mostly it is running great, however I get strange artifacts on mostly only the front side of curved objects.

I have lubed all the rods, and I have a Capricorn PTFE tube from the filament sensor to the hot end. I tried the printable guide for the tube to go into the hot end but it wasn't any better and I thought that was the culprit at first.

I have an extension piece to raise up the top glass.

I'm using Elegoo Rapid PTEG running at 240c and 250mm outerwall speed. This is mainly happening on the front side and anywhere on the build plate. Filament is dry and fed out of the Creality Space dryer.

These items are small netcups but it was also happening on the larger sections that they go in.

Using Orcaslicer and Arachne wall generator.

Any ideas where I need to be focusing my attention on?

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 1 points 1 month ago

I re-lubed the rods before starting another set and still having the issue. I was thinking it had something to do with the Bowden tube but even at the back where the tube doesn't move much the issue still happens.

Is there a specific lube that is better than others?