this post was submitted on 18 Feb 2024
23 points (96.0% liked)

3DPrinting

15138 readers
14 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: [email protected] or [email protected]

There are CAD communities available at: [email protected] or [email protected]

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

I am somewhat new to 3d printing and i am playing around with different filaments and print plates on my cheap ender3 v3 se.

Right now I am observing a weird adhesion-issue i have not seen before: The copper-silk filament has trouble sticking to the printplate, but only in some places of the plate.

My guess it's either some dirt/oil on the printplate. Or maybe the silk-pla has bad adhesion.

What do you think?

This printplate is this (but glued over the original printplate): https://www.amazon.de/dp/B0CL5FYHBR

The filament is this: https://www.amazon.de/dp/B09CPBRQXS

some clarification for the video: all corners of the first layer should have been rectangular. Instead some corner lost adhesion and become roundish. Here is the view from the slicer: https://imgur.com/rwA0fQW

you are viewing a single comment's thread
view the rest of the comments
[–] [email protected] 8 points 6 months ago* (last edited 6 months ago) (2 children)
  1. Try increasing hotend temp for first few layers and hotbed temp throughout
  2. Try moving z closer for first layer
  3. Repeat both of above in small increments

FWIW, those PEI sheets usually need higher bed temp than the regular sheets

[–] [email protected] 2 points 6 months ago (1 children)

Try increasing hotend temp for first few layers and hotbed temp throughout

the default from the printer was 60C. I had some better results with 70C. But the issue still happend with more delicate prints.

those PEI sheets usually need higher bed temp than the regular sheets

thanks. I didn't know that. What magnitude are we talking here (like: 10K more for PEI-sheets? or more like 1K?)

Try moving z closer for first layer

I think this may be the solution. How much should I change the z-offset? (the print in the video has 0.2mm layer height. And the worst-adhession issues happened with 0.1mm)

[–] [email protected] 5 points 6 months ago

K Kelvin, not K thousands of degrees... It's too early to think.

You may also have a bed flatness problem, if it's not a dirty plate.